Product Dose

Using Procedure and operting data :

  Spray or Power Wash Immersion Electrolytic
Concentration 10 – 30 ml/L 50 – 150 ml/L 50-150ml/L
Temperature 40 – 80°C 40 – 80°C 40 – 80°C
Time 0.5 – 3 mins 2 – 5 mins 1 – 5 mins
Current Density
(Ferrous, Anodic)
    2.5 – 10A/dm²
(Non-ferrous,
cathodic)
    5.0 – 7.5 A/dm²
 

Soak Clean Eco Manufacturer

Soak Clean Eco Exporter

Soak Clean Eco Supplier